Electrolysis in an aqueous medium with direct current normally produces off-gassing at both electrodes (hydrogen at the cathode, oxygen at the anode). However, if aluminum is used as the anode, no off-gassing is observed at the anode, while hydrogen is always visible at the cathode.
To a first approximation, this phenomenon can be described as a combination of dissolved aluminium and nascent oxygen, according to the reaction :
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
(1) - SMELTZER (W.W) - Principles applicable to the oxidation and corrosion of metals and alloys. - Corrosion, vol. 11, 366 t-374 t (1995).
(2) - VARGEL (C.) - Corrosion de l'aluminium. - Éd. Dunod, p. 87 (1999).
(3) - WEFERS (K.) - Aluminium. - 57,...
Also in our database
DEVELAY (R.) - Propriétés technologiques de l'aluminium et ses alliages corroyés. -
Standards
Anodizing aluminum and its alloys – Determination of mass per unit area (mass per unit area) of anodic layers – Gravimetric method. - • NF EN ISO 2106 - Avril 2011
Anodizing aluminum and its alloys – Determining the thickness of anodic layers – Non-destructive method using an optical sectioning microscope. - • NF EN ISO 2128 - Octobre 2010
Non-conductive coatings on non-magnetic base metal – Thickness measurement...