5. Effect of heat treatment on electroless nickel-boron coatings
As expected, electroless nickel-boron coatings without special treatment show a metastable structure that does not correspond to that predicted by the nickel-boron phase diagram for these boron contents. This is because the solubility of boron in nickel at room temperature is extremely low, and numerous intermetallic compounds (such as Ni2B, Ni3B, Ni4B3...) can be formed as a function of the boron content of the mixture . The hardness of these borides, some of which have crystal structures similar to hard phases such as cementite, is high....
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
Effect of heat treatment on electroless nickel-boron coatings
Bibliography
-
(1) - RIEDEL (W.) - Electroless nickel plating. - Finishing Publication LTD., London, OH (1989).
-
(2) - OHNO (I.) - Electrochemistry of electroless plating. - Mater. Sci. Eng. A. 146 33-49. doi :10.1016/0921-5093(91)90266-P (1991).
-
(3) - VITRY (V.) - Electroless...
Also in our database
-
BOTTARI (P.), ROBIN (F.), PARKINSON (R.) - Dépôts de nickel chimique – Applications. - [M 1 567]...
Regulations
ELV (End of Life Vehicles).
European Directive 2000/53/EC on end-of-life vehicles stipulates that "materials and components for vehicles put on the market after 1er January 2003 must not contain lead, cadmium, mercury or hexavalent chromium. The tolerance is 0.1% for lead and 0.01% for cadmium, provided that these substances are not intentionally introduced."
RoHS (Restriction of Hazardous Substances).
The...
Patents
Mc Comas, E. Nodular nickel boron coating, US patent N° 20040111947, 2004. (Universal Chemical Technologies Inc., Florida.
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!