6. Specificity of high-alloy cast irons
European standard NF EN 12513 (White irons resistant to abrasive wear) contains an informative annex on the heat treatment of nickel-chromium cast irons on the one hand, and high-chromium cast irons on the other.
SCROLL TO TOP
6.1.1 Nickel-chromium cast irons
These grades can benefit from a stress-relieving heat treatment at 275°C for 8 to 16 hours, followed by either air or furnace cooling.
To increase resistance to repeated impacts, castings with 4% nickel and 2% chromium can be tempered at 450°C...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
Specificity of high-alloy cast irons
Bibliography
References
-
(1) - Manuel des fontes moulées, - traduit et adapté de Iron Castings Handbook par le CIFOM. Éditions techniques des Industries de la Fonderie (566 p., 194 tabl., 444 fig.) (1983).
-
(2) - SY (A. de), VIDTS (J.) - Traité de métallurgie structurale théorique et appliquée. - 510 p., DUNOD/NICI...
Standardization
- Foundry – Designation system for cast iron. Symbolic and numerical designation. Replaces NF A 02-001. - NF EN 1560 - 09-97
- Foundry – Lamellar graphite cast iron. Replaces NF A 32-101. - NF EN 1561 - 10-97
- Foundry – Malleable cast iron. Replaces NF A 32-701 and NF A 32-702. - NF EN 1562 - 10-97
- Foundry – Spheroidal graphite cast iron. Replaces NF A 32-201. - NF EN 1563 - 10-97
- Foundry – Cast...
Organizations
Association technique de fonderie (ATF)http://www.atf.asso.fr/
Association technique de traitement thermique (ATTT)http://www.attt.org/
Centre technique des industries de la fonderie (CTIF)http://www.ctif.com/