2. Stress relief and softening treatments

2.1 Softening treatments

The purpose of softening treatments is to facilitate the deformation of materials during forming operations or to facilitate machining.

When the material has previously been work-hardened, the level of treatment should enable restoration or recrystallization. In concrete terms, the effectiveness of this treatment will mainly depend on the solutionization of the hardening phase (γ ' or γ″) and, if possible, the carbides, as these constituents increase the material's strength and therefore limit deformability.

The temperatures and times to be used are similar to those for solution setting. However, certain precautions should be taken when...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Ongoing reading
Stress relief and softening treatments

Article included in this offer

"Metal treatments"

( 136 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details
Contact us