Fractography practice
Fractography - Break morphology

Add to my library

M4121 V1 Article

Fractography practice
Fractography - Break morphology

Authors : Annick POKORNY , Jean POKORNY

Publication date: December 10, 2002 | Lire en français

Add to my library Add to my library

Logo Techniques de l'Ingenieur You do not have access to this resource.
Request your free trial access! Free trial

Already subscribed?

2. Fractography practice

2.1 As soon as a breakup is announced

It would be a good idea to visit the site to record all the objects in their environment.

As with archaeological and other types of expertise, you could say "hurry up and don't touch anything", because you have to leave yourself the possibility of going back: from the outset, the "sampling" has to be beyond reproach.

If the debris is scattered, all the pieces must be found, at least one of the halves bearing the original primer:

  • in the case of exploded tubes or tanks, it is necessary to examine the probable chevrons, over metres of fracture;

  • in the case of cascading failures of a machine, such as a crash, we look for the fatigue crack (which necessarily predates the other failures), but we still...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Article included in this offer

"Studies and properties of metals"

( 199 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details
Contact us