3. Superalloy metallurgy
The metallographic structure of a superalloy is made up of several phases .
An austenitic γ matrix with a face-centered cubic structure (cfc) in which the elements Co, Cr, Mo, W and, to a lesser extent, Nb, Al, Ti and Ta can be substituted for Ni. These elements provide hardening in solid solution (figure 7).
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
Superalloy metallurgy
Bibliography
Bibliography
-
(1) - KRACKE (A.) - Superalloys, the most successful alloy system of modern times – Past, present and future. - 7th International symposium on superalloys 718 and Derivatives, p. 13, TMS (The minerals, Metals and Materials Society) (2010).
-
(2) - HEANEY (J.A.), LASONDE (M.L.), POWELL (A.M.),...
Also in our database
-
MONS (C.) - Traitement thermique des superalliages. - [M 1 165] (2009).
- ...
Events
International Symposium on Superalloys. Seven Springs. USA. International conference on superalloys, held every 4 years. TMS (The minerals, Metals and Materials Society) http://www.tms.org
International Symposium on Superalloys 718 and Derivatives. Pittsburgh, USA. Conference on 718 superalloys and derivatives held every 4 years in the United States. TMS (The Minerals,...
Directory
Documentation – Training – Seminars (non-exhaustive list)
Proceedings of the International Symposium on Superalloys (Seven Springs) (1968-1972-1976-1980-1984-1988-1992-1996-2000-2004-2008-1012-2016- 2020)
Proceedings of the International symposium on superalloys 718 and Derivatives (1989-1991-1994-1997-2001-2005-2010-2014-2018)
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!