4. Conclusion

Fractures are the result of superimposed stresses and brittle materials.

Corrosion plays a special role here: it can occur without any external force, but with internal stresses, always combined with a mechanical weakness in the metal; it can also occur without any mechanical stress, in which case it is due to a local or general electrochemical weakness in the metal.

In virtually all cases, the macrographic and micrographic surface finish is predominant.

The synthesis of these factors can be seen in the relief of the break, an image of actual past events (see articleFractography. Morphology of fractures ).

SCROLL TO TOP
You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Ongoing reading
Conclusion

Article included in this offer

"Studies and properties of metals"

( 174 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details
Contact us