5. Illustrative results on the effectiveness of polymer-silver composite film
In the example presented here, the operating conditions chosen for plasma treatment (argon pressure = 40 mTorr, HMDSO flow rate = 0.1 sccm, P
HMDSO
= 2.5 mTorr, I
Ag
/ I
Ar
= 0.20) resulted in a composite film comprising 25% silver. The corresponding yeast detachment profile is shown in figure
10
. Control" profiles, obtained with baker's yeast previously adhered to virgin stainless steel and coated...