Specificity of high-alloy cast irons
Heat treatment of cast iron

Add to my library

M1145 V4 Article

Specificity of high-alloy cast irons
Heat treatment of cast iron

Authors : Simone PARENT-SIMONIN, Jean-Claude MARGERIE

Publication date: December 10, 2001 | Lire en français

Add to my library Add to my library

Logo Techniques de l'Ingenieur You do not have access to this resource.
Request your free trial access! Free trial

Already subscribed?

6. Specificity of high-alloy cast irons

6.1 White carbide cast irons

European standard NF EN 12513 (White irons resistant to abrasive wear) contains an informative annex on the heat treatment of nickel-chromium cast irons on the one hand, and high-chromium cast irons on the other.

SCROLL TO TOP

6.1.1 Nickel-chromium cast irons

These grades can benefit from a stress-relieving heat treatment at 275°C for 8 to 16 hours, followed by either air or furnace cooling.

To increase resistance to repeated impacts, castings with 4%...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Ongoing reading
Specificity of high-alloy cast irons

Article included in this offer

"Metal treatments"

( 131 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details
Contact us