3. Applications
The examples given below are by no means an exhaustive list of DSC applications.
Differential scanning calorimetry can be used to determine enthalpy variations, including those corresponding to first-order transitions in the Erhenfest sense.
SCROLL TO TOP
3.1.1 Enthalpy variation between two temperatures
When there is no phase change between two temperatures, the enthalpy variation is obtained by the heat capacity measurement method:
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
Applications
Bibliography
(1) - CALVET (E), PRAT (H.) - Microcalorimétrie, applications physico-chimiques et biologiques. - Masson, Paris (1956).
(2) - CLAUDY (P.) - Analyse calorimétrique différentielle. - Lavoisier, ISBN : 2-7430-0716-8 (2005).
(3) - OLLIVON...
Standards and norms
The international standard ISO (International Standardisation Organisation) is recommended but not mandatory.
The European standard (EN) is mandatory. It replaces the equivalent national standard.
The French standard (NF) applies in the absence of other European or international standards.
Differential Scanning Calorimetry for plastics is covered by ISO 11357 (also EN and NF standards). It is divided into...
Directory
Associations French Association for Calorimetry and Thermal Analysis http://www.afcat.org
International Conference for Thermal Analysis and Calorimetry http://www.ictac.org
European Virtual Institute for Thermal Metrology http://www.evitherm.org
...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!