2. The different stages of solid phase sintering
Consider a mole of copper (63.5 g), made up of 1 µm cubic grains, and the same mole of copper made up of a single grain (figure
7
). These two systems differ in the areas of their solid-gas interfaces. The single grain has a lower specific surface area (surface area per unit mass) than the dispersed system. This decrease in surface area d A
sg
corresponds to a decrease in energy of the form γ
sg
d A
sg
. The proportionality coefficient γ
sg
is...