3. Steel corrosion mechanisms
During the mixing of Portland cement-based concrete, the main anhydrides contained in the clinker (silicates C2S and C3S, aluminates C3A and C4AF) hydrate on contact with water [C 920]. From the very first moments, a very basic pH of around 13.5 to 14 can be measured in the interstitial liquid.
Schematically, the hydration of C2S and C3S leads to the formation of...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
Steel corrosion mechanisms
Bibliography
-
(1) - MANCIO (M.), ZHANG (J.), MONTEIRO (P.J.M.) - Non-destructive surface measurement of corrosion of reinforcing steel in concrete, National Research Council Canada, NRCC-47296 - Canada (2004).
-
(2) - LAFERRIERE (F.) - Surveillance des ouvrages de génie civil par capteurs à fibres optiques : capteurs d'ions chlore - École...
Also in our database
-
BAROGHEL-BOUNY (V.) - Nouvelle approche de la durabilité du béton. Méthodologie et exemples -
Standards and norms
- Standard Test Method for half-cell potentials of uncoated reinforcing steel concrete, ASTM Standard, section 4, vol. 04.02, Cement and Aggregates. - ASTM C876-91 - 1999
- European standard: concrete – Part 1: Specifications, performance, production and conformity, AFNOR, et Dispositions Nationales. - EN 206-1 - jan. 2000
- Norme Européenne : Eurocode 2 : Calcul des structures en béton et Document d'application...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!