Overview
ABSTRACT
This article introduces superalloys, whose history evolves in parallel with that of aeronautics. By explaining the metallurgy of superalloys, from their chemical composition to their role in the aging principle, this presentation details the main manufacturing processes: vacuum melting followed by remelting under vacuum or under slag protection for conventional forged or rolled alloys; vacuum atomization and consolidation by extrusion and isothermal forging for alloys from powder metallurgy; investment casting applied to polycrystalline, directional solidification and monocrystalline superalloys; conversion; heat treatment; non destructive inspection.
Read this article from a comprehensive knowledge base, updated and supplemented with articles reviewed by scientific committees.
Read the articleAUTHOR
-
Philippe HERITIER : Senior metallurgist - Former Technical Director (Research & Development, Metallurgical Services, Application Engineering) at Aubert & Duval, Clermont Ferrand, France
INTRODUCTION
The term "superalloys" is generally reserved for austenitic alloys which, when used at high temperatures in excess of 500°C, exhibit exceptional mechanical properties:
mechanical strength ;
tenacity ;
creep resistance ;
resistance to oxidation and corrosion ;
structural stability.
There are three families of superalloys:
nickel-based alloys ;
iron-nickel base alloys ;
cobalt-based alloys.
The development of superalloys has been largely based on innovations in alloy chemistry and manufacturing processes. It has mainly been driven by the aerospace and energy industries.
If superalloys have been so successful, it's because they have met the pressing demands of in-service properties. A century ago, generating such power in machines and propulsion systems was scarcely imaginable. Superalloys have helped us conquer air and space, reach the depths of the earth and the ocean, and meet many other challenges of modern life.
As such, they deserve to have their story told, their metallurgy explained and their use illustrated. But it's not an easy task. The evolution of this industry has unfolded through a multitude of small and large events, a multitude of more or less important inventions, at the crossroads of borders, nations and diverse industries. So many people have contributed to the state of the art in 2022, that the light we're going to try to shed on it is bound to be imperfect. But it will be as exhaustive as possible.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!
KEYWORDS
aeronautics | melting | vacuum | superalloys | | Single crystals
Superalloys
Bibliography
Bibliography
Also in our database
Events
International Symposium on Superalloys. Seven Springs. USA. International conference on superalloys, held every 4 years. TMS (The minerals, Metals and Materials Society) http://www.tms.org
International Symposium on Superalloys 718 and Derivatives. Pittsburgh, USA. Conference on 718 superalloys and derivatives held every 4 years in the United States. TMS (The Minerals,...
Directory
Documentation – Training – Seminars (non-exhaustive list)
Proceedings of the International Symposium on Superalloys (Seven Springs) (1968-1972-1976-1980-1984-1988-1992-1996-2000-2004-2008-1012-2016- 2020)
Proceedings of the International symposium on superalloys 718 and Derivatives (1989-1991-1994-1997-2001-2005-2010-2014-2018)
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!
Article included in this offer
"Design and engineering management"
(
367 articles
)
Updated and enriched with articles validated by our scientific committees
A set of exclusive tools to complement the resources