3. The different stages of plastic welding
Moisture recovery
Some materials have moisture absorption properties, which means that if you weld them at high ambient humidity, there's a risk that the water contained in the material will vaporize. Depending on the type of material, this translates into :
small surface craters for PMMA (polymethyl methacrylate),
white foam for PCs (polycarbonate),
the impossibility of welding PA (polyamide), etc.
Check this parameter by studying the material's technical data sheet: result of a water absorption test at 23°C for 24 hours with a specified percentage of humidity or saturation: x gram of water absorbed in 24 hours.
Compare safe materials like PP (polypropylene) and PE (polyethylene)...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
The different stages of plastic welding
Bibliography
Also in our database
-
(1) - La soudure des thermoplastiques par air chaud sans apport de matière externe -
Regulatory references
NF EN 13067: December 2012 — Plastics welding personnel — Welder qualification test — Thermoplastic welded assemblies
AFG B.527.9 : According to the specifications of the French Gas Association, qualification test for polyethylene operators.
Products and suppliers
Would you like to be trained in plastic welding techniques, material assembly and boiler making? Do you need contacts for QS and QMOS validation? Contact Techniques de l'Ingénieur on 01 53 35 20 25 or by email: [email protected]