1. Part quality and casting defects
The quest for part quality involves identifying anomalies or defects that may occur during the casting process. These defects or anomalies may originate from :
part design and layout ;
choice of molding technology ;
design of models and/or molds ;
definition of filling and feeding systems;
alloy production and liquid metal processing conditions;
finishing, heat treatment or surface treatment operations.
In fact, the success of a cast part is always the result of the right combination of properties specific to the chosen process and alloy. These strong alloy/process interactions sometimes make it difficult to diagnose the origins of observed...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!
Ongoing reading
Part quality and casting defects
Bibliography
-
(1) - - Recherche de la qualité des pièces de fonderie – Éditions techniques des Industries de la Fonderie (1986).
-
(2) - JACOB (S.), FONTAINE (D.) - Brûlure de l'A-U5GT au cours du traitement thermique - Fonderie n° 294, p. 326-336 (1970).
-
(3)...
Also in our database
-
CAZES (R.) - Soudage à l'arc - [B 7 730] Génie mécanique (1995).
- ...
Brochures and catalogs
Éditions Techniques des Industries de la Fonderie catalog and Centre Technique des Industries de la Fonderie brochures.
International bibliographic databases
Aluminium Metadex
Reviews
France
Fonderie magazine (CTIF and ATF, monthly)
Revue de Métallurgie (monthly)
Germany
Gießerei (monthly)
Gießerei-Praxis (monthly)
Gießerei Forschung (quarterly)
United States
Modern Casting (monthly)
Foundry Management and Technology (monthly)
Die Casting Engineer (bimonthly)
Advanced Materials and Processes (monthly)
Materials Engineering (monthly)
...
Exhibitions and congresses
World
World Foundry Congress: every two years in a different country, usually at the end of the 3rd quarter.
France
Journées d'Études de l'Association Technique de Fonderie (ATF): in France, every year.
SF2M annual days organized by the French Society of Metallurgy and Materials: every year in October.
United States
Annual spring meeting of American Foundrymen organized by the...
Patents
French National Institute of Industrial Property (INPI)
A large number of patents relating to aluminum alloy casting have been filed or are in the process of being filed around the world; an exhaustive list is virtually impossible to compile due to the constant filing of new patents, which means that they have to be constantly updated.
To obtain information on a given subject at a given time, it is therefore advisable to contact...
Standardization
French and European standards. French Standards Association (AFNOR)
http://www.afnor.org
Standards NF EN ISO
- Geometric product specification (GPS) – Dimensional and geometric tolerances for molded parts. - NF EN ISO 8062 - (2007) :
NF EN standards
- Aluminium and aluminium alloys – Master alloys obtained by melting – Specifications....
Theses
http://www.sudoc.abes.fr
BRACCINI (M.). – Optimization of castings: study of hot cracking phenomena in Al-Cu alloys. INP Grenoble (2000).
SAVELLI (S.). – Identification of mechanisms and quantitative approach to fatigue of cast aluminum model alloys. INSA Lyon (2000).
EVANS (W.J.), JONES (H.V.), SPITTLE (J.A.) and BROWN (S.G.R.). – "Defect sensitive...
You do not have access to this resource.
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed?
Log in!