5. Oxidation – Corrosion

Zirconium alloys and hafnium resist well in water and steam under nuclear reactor operating conditions, at around 300°C. The oxide layers formed reach a few tens of microns, rarely more than 100 µm, after 3 to 6 years (under neutron irradiation).

  • In air, oxidation is highly temperature-dependent, as shown in table 3 . The oxide layer is protective at low thicknesses (typically 3-10 µm), but degrades beyond that. For this reason, zirconium can be used at low temperatures (below 400 or 500°C), but oxidizes rapidly at higher temperatures. Nitriding only takes place above 800°C, when oxygen pressure is low.

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Article included in this offer

"Studies and properties of metals"

( 175 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details
Contact us