3.1.1 Hot strip scale structure
It should be remembered that we are only studying the case of low-carbon mild steel strips that have a self-annealed structure after hot rolling.
The cold structure of the pickled scale normally differs from the hot structure, as FeO is unstable below 570°C.
-
Hot structure
Virtually all mill scale is formed at high temperature, in contact with air, between the outlet of the last...