2. Properties

2.1 Structure

PBT and PET are semi-crystalline polymers (in the solid state, part of the material is amorphous and the rest is crystallized).

The crystallinity rate does not exceed 40-50% by volume. A number of factors influence the rate of crystallization:

  • the chemical nature of the polymer: PBT crystallizes much faster than PET ;

  • the molecular weight of the polymer: the higher the molecular weight, the lower the crystallization rate;

  • temperature.

For PET, the crystallization rate is highest at around 175 C. Still sufficient between 130 and 140 C to enable molding cycle times of less than 1 min, it becomes...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Article included in this offer

"Plastics and composites"

( 347 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details
Tous les livres blancs
Toutes les actualités
Contact us