5. Conclusion

Although already patented in 1977 at the same time as temporal ALD, spatial ALD was only developed at the beginning of the 21st century. The possibility of using ALD at higher deposition rates, at atmospheric pressure (and even in the open air), has focused attention on SALD with a strong development momentum. Since the first publications in 2004 and 2008, the number of publications has grown steadily. SALD has also made the transition from laboratory to industrial scale, and several commercial systems are already available for both laboratory and production use.

SALD is a highly flexible deposition technology that allows great freedom of design, as demonstrated by the growing number of reactors currently under development. Because precursors are continuously injected into the SALD, efficient separation by the gas/inert zone flow must be ensured. Analytical fluid...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Article included in this offer

"Nanosciences and nanotechnologies"

( 137 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details

Dans les ressources documentaires

Réacteurs ALD

Les réacteurs de dépôt de couche minces par ALD (Atomic Layer Deposition) pour une variété d'applications...

Encapsulation des diodes organiques électroluminescentes et microbatteries par ALD

Le problème des diodes électroluminescentes organiques (OLED) et des microbatteries à base d’une technolo...

Dépôt par ablation laser pulsé

Cet article est une revue de la technique de dépôt en couche mince par ablation laser pulsé ou  Puls...

ALD en microélectronique - Applications, équipements et productivité

Cet article est une revue de l’utilisation du dépôt par couches atomiques dans le secteur de la microélec...

Tous les livres blancs
Article Qu'est-ce que le Power-to-Gas ?
1 September 2023
Qu'est-ce que le Power-to-Gas ?

Le Power-to-Gas est le procédé par lequel de l’énergie électrique est convertie en énergie chimique, sous forme gazeuse. Par rapport à l’électricité, le gaz ain...

Toutes les actualités
Contact us