10. Relationships between structures and properties

Cobalt-based superalloys are mainly solid solution hardened. Their strength is not comparable to that of nickel-based superalloys. The latter, or iron-nickel-based superalloys used for the most critical applications, are hardened by γ' or γ'' precipitation in a face-centered cubic matrix, itself hardened by solid solution. The atomic percentage of γ' phase varies from 20 to 40% for conventional wrought alloys, and from 40 to 60% or even more for alloys obtained by powder metallurgy or casting.

The microstructure of components of a given chemistry is the result of the manufacturing process: elaboration, casting, forging, stamping, heat treatment, etc. The end of the process, and particularly the heat treatment, enables us to find the optimum properties in relation to the use of the component. The end of the process, and more specifically the heat treatment, enables...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Article included in this offer

"Functional materials - Bio-based materials"

( 201 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details

Dans les ressources documentaires

Propriétés des alliages d’aluminium de fonderie

La fonderie d’aluminium a connu un développement remarquable dans l’industrie automobile, en raison des t...

Traitements thermiques des alliages de zirconium et de hafnium

Les traitements thermiques des alliages de zirconium et de hafnium font partie intégrante du procédé de t...

Molybdène et alliages

Karl Wilhelm Scheele mettait fin, en 1778, à la confusion qui régnait sur la nature de la molybdénite et ...

Traitements thermiques du cuivre et de ses alliages

Les traitements thermiques ont pour but, d’une part, de permettre la transformation des produits en homog...

Tous les livres blancs
Toutes les actualités
Contact us