1. History

The term "superalloys" was coined in the mid-1940s. This term defined the quality of high-temperature alloys that could not only be used at high temperatures, but also retained their strength and toughness at the same temperatures. Applications included the development of gas turbine engines for military aircraft.

In November 1919, at the International Nickel Company's research laboratory in Bayonne (NJ, USA), a note was placed on Paul Merica's desk requesting the development of a stronger Monel ® (nickel-copper alloy family). The target application was steam turbine blades. The practice at the time was to melt a series of castings with different chemical compositions in order to determine which matched the desired effect. Aluminum levels in the castings were increased by up to 5%. This work was the first of its kind...

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Article included in this offer

"Studies and properties of metals"

( 172 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details

Dans les ressources documentaires

Propriétés des alliages d’aluminium de fonderie

La fonderie d’aluminium a connu un développement remarquable dans l’industrie automobile, en raison des t...

Traitements thermiques des alliages de zirconium et de hafnium

Les traitements thermiques des alliages de zirconium et de hafnium font partie intégrante du procédé de t...

Molybdène et alliages

Karl Wilhelm Scheele mettait fin, en 1778, à la confusion qui régnait sur la nature de la molybdénite et ...

Traitements thermiques du cuivre et de ses alliages

Les traitements thermiques ont pour but, d’une part, de permettre la transformation des produits en homog...

Tous les livres blancs
Toutes les actualités
Contact us