Controlling the quality of castings is an absolute imperative for both suppliers and users. This article summarizes the typical defects and their remedies, the rules of the design of parts and tools as well as the potential of the numerical simulation of filling and solidification, which has become a major tool for quality in casting.

Read this article from a comprehensive knowledge base, updated and supplemented with articles reviewed by scientific committees.

Read the article

AUTHORS

  • Michel GARAT : ESPCI engineer, private consultant, former R & D director of Aluminium Pechiney casting alloys and project manager Rio Tinto Alcan, Peyrins, France

  • André LE NÉZET : ESF engineer, non-ferrous alloys casting expert, Renault, Rueil-Malmaison, France

 INTRODUCTION

The quality of a cast part can be defined as its ability to satisfy the requirements specified in the customer's specifications. It depends on the design of the part by the client, and on the care taken in its production by the caster, who must master a large number of manufacturing parameters.

One of the keys to achieving this quality is to recognize and describe any anomalies or defects that may occur during the casting process, so that corrective action can be taken. Defects observed in aluminum alloy castings are similar to those encountered with other metals and alloys, though with some specific features, such as their high oxidizability in the liquid state and their tendency to dissolve hydrogen. These defects are examined in the first part of the article.

Part design must take into account the casting process used. The diversity of these processes in the case of aluminum alloys implies certain basic rules, the correct application of which is a prerequisite for obtaining quality parts. Digital techniques known as "virtual prototyping", which range from dimensional calculation to simulation of filling, solidification and cooling, enable improved part design and quality, as well as a significant reduction in costs and development times. This article describes the different types of defects and their origins, the means of repair, the design rules for avoiding them, and concludes with a discussion of numerical simulation of foundry processes, a major tool for rapidly achieving satisfactory quality.

The following articles complete the subject:

  • [M 3 635] – Aluminium alloy melting ;

  • [M 3 636] – Aluminum alloy casting. Sand, investment casting and visible processes;

  • [M 3 637] – Aluminum alloy casting. Permanent molds: shell, die-cast and related.

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Ongoing reading
Casting of aluminum alloys -Defects and part design

Article included in this offer

"Metal forming and foundry"

( 124 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details

Dans les ressources documentaires

Fonderie et moulage des alliages de cuivre

Les alliages cuivreux moulés nous accompagnent tous les jours. Dans cet article, sont présentés la grande...

Diagrammes d’équilibre - Alliages binaires

Un alliage peut exister sous différents états : solide cristallisé , en agrégat de microcristaux appelés...

Effet thermique de la mise en forme - Phénomènes superficiels

L’évolution thermique superficielle du métal mis en forme et des outils conditionne la qualité superficie...

Tous les livres blancs
Toutes les actualités
Contact us