ABSTRACT

This article firstly presents the basis of the differential scanning calorimetry with sinusoidally modulated temperature (TMDSC). It details the various signals registered during experiment (excitement, calorimetric response) as well as the various magnitudes (invertible or non-invertible flux, thermal capacity) derived from the deconvolution of these registered signals. It also deals with certain method issues (phase correction, influence of frequency) and presents some examples illustrating the expected advantages of this method as well as related calorimetric methods (Step-Scan® et TOPEM®).

Read this article from a comprehensive knowledge base, updated and supplemented with articles reviewed by scientific committees.

Read the article

AUTHORS

  • Jean GRENET : Professor Emeritus - LECAP Laboratory EA 4528, Institute for Material Research FED 4114, University of Rouen

  • Bernard LEGENDRE : Professor Emeritus - Materials and Health Laboratory, EA 401, Faculty of Pharmacy Paris 11

 INTRODUCTION

As early as the beginning of the 20th century, researchers came up with the idea of using a non-linear variation in temperature for the duration of the calorimetric analysis. This idea was supported by the desire to be close to equilibrium, or to separate phenomena whose kinetics may be similar. The current answer to these concerns is provided by temperature-modulated DSC.

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


Ongoing reading
Differential scanning calorimetry with modulated temperature (TMDSC)

Article included in this offer

"Analysis and Characterization"

( 271 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details

Dans les ressources documentaires

Caractérisation des polymères par analyse thermique

L‘analyse thermique englobe toute une série de techniques de caractérisation des matériaux fondées sur l’...

Mesure de l’effusivité thermique - Méthodes par contact

Sont recensés deux types de méthodes de contact, selon la manière dont la perturbation thermique est assu...

Microcalorimétrie à balayage DSC - Application agroalimentaire

La microcalorimétrie différentielle en programmation linéaire de température ou Differential Scanning Cal...

Compteurs de volume de gaz - Partie 2

Cet article concerne l’ensemble des compteurs de volume de gaz en fonction de la température et de la pre...

Tous les livres blancs
Toutes les actualités
Contact us