9. Finishing: non-destructive testing, machining, welding
9.1 Non-destructive testing
Non-destructive testing (NDT) is a set of methods for characterizing the integrity of structures or materials, without damaging them, either during production, use or maintenance. When it comes to superalloys, one of the difficulties lies in controlling the cleanliness of alloys, i.e. the level of inclusions (oxides, nitrides, carbonitrides) or defects generated by these inclusions during manufacturing processes (vacuum induction furnace + remelting or vacuum atomization + consolidation). These inclusions, whose existence is inherent to manufacturing processes, are in fact sources of crack initiation during cyclic loading (fatigue).
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!
Finishing: non-destructive testing, machining, welding
Article included in this offer
"Design and engineering management"
(
347 articles
)
Updated and enriched with articles validated by our scientific committees
A set of exclusive tools to complement the resources
Bibliography
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!