Superalloys

Add to my library

M4770 V1 Article

Superalloys

Author : Philippe HERITIER

Publication date: July 10, 2022 | Lire en français

Add to my library Add to my library

Logo Techniques de l'Ingenieur You do not have access to this resource.
Request your free trial access! Free trial

Already subscribed?

Overview

ABSTRACT

This article introduces superalloys, whose history evolves in parallel with that of aeronautics. By explaining the metallurgy of superalloys, from their chemical composition to their role in the aging principle, this presentation details the main manufacturing processes: vacuum melting followed by remelting under vacuum or under slag protection for conventional forged or rolled alloys; vacuum atomization and consolidation by extrusion and isothermal forging for alloys from powder metallurgy; investment casting applied to polycrystalline, directional solidification and monocrystalline superalloys; conversion; heat treatment; non destructive inspection.

Read this article from a comprehensive knowledge base, updated and supplemented with articles reviewed by scientific committees.

Read the article

AUTHOR

  • Philippe HERITIER : Senior metallurgist - Former Technical Director (Research & Development, Metallurgical Services, Application Engineering) at Aubert & Duval, Clermont Ferrand, France

 INTRODUCTION

The term "superalloys" is generally reserved for austenitic alloys which, when used at high temperatures in excess of 500°C, exhibit exceptional mechanical properties:

  • mechanical strength ;

  • tenacity ;

  • creep resistance ;

  • resistance to oxidation and corrosion ;

  • structural stability.

There are three families of superalloys:

  • nickel-based alloys ;

  • iron-nickel base alloys ;

  • cobalt-based alloys.

The development of superalloys has been largely based on innovations in alloy chemistry and manufacturing processes. It has mainly been driven by the aerospace and energy industries.

If superalloys have been so successful, it's because they have met the pressing demands of in-service properties. A century ago, generating such power in machines and propulsion systems was scarcely imaginable. Superalloys have helped us conquer air and space, reach the depths of the earth and the ocean, and meet many other challenges of modern life.

As such, they deserve to have their story told, their metallurgy explained and their use illustrated. But it's not an easy task. The evolution of this industry has unfolded through a multitude of small and large events, a multitude of more or less important inventions, at the crossroads of borders, nations and diverse industries. So many people have contributed to the state of the art in 2022, that the light we're going to try to shed on it is bound to be imperfect. But it will be as exhaustive as possible.

You do not have access to this resource.
Logo Techniques de l'Ingenieur

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource. Click here to request your free trial access!

Already subscribed?


KEYWORDS

aeronautics   |   melting   |   vacuum   |   superalloys   |     |   Single crystals

Ongoing reading
Superalloys

Article included in this offer

"Design and engineering management"

( 347 articles )

Complete knowledge base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

View offer details

Dans les ressources documentaires

Propriétés des alliages d’aluminium de fonderie

La fonderie d’aluminium a connu un développement remarquable dans l’industrie automobile, en raison des t...

Traitements thermiques des alliages de zirconium et de hafnium

Les traitements thermiques des alliages de zirconium et de hafnium font partie intégrante du procédé de t...

Molybdène et alliages

Karl Wilhelm Scheele mettait fin, en 1778, à la confusion qui régnait sur la nature de la molybdénite et ...

Traitements thermiques du cuivre et de ses alliages

Les traitements thermiques ont pour but, d’une part, de permettre la transformation des produits en homog...

Tous les livres blancs
Toutes les actualités
Contact us