6. Creep associated with oxidation and/or fatigue phenomena
In rotating machines such as gas turbines or aeronautical turbomachines, creep is combined with either oxidation or fatigue (cyclic mechanical stress), or often both.
6.1 Effect of oxidizing atmosphere on creep behaviour
The two main oxidation phenomena are :
the creation of a protective layer by the formation of a more or less stable compound (generally oxides) with one or more elements from the atmosphere; if the compound is desquamated, the cross-section of the material subjected to stress decreases, the stress exerted increases and therefore the rate of deformation increases; but if the compound is stable and forms a continuous film on the surface of the material, the rate of deformation decreases because part...
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!
Creep associated with oxidation and/or fatigue phenomena
Article included in this offer
"Studies and properties of metals"
(
172 articles
)
Updated and enriched with articles validated by our scientific committees
A set of exclusive tools to complement the resources
Bibliography
References
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!