1. General
1.1 Performing a creep test
A creep test is broken down into two stages (figure 1 ): loading and creep.
In practice, it's not always easy to carry out a constant stress test. Indeed, if the deformation is significant, the test is carried out at constant force: the stress increases during the test with the elongation of the specimen (figure 1 ). The creep test is defined by standard NF A 03-355.
Depending on the materials and equipment used during the test, numerous precautions need to be taken. In particular, for a high-temperature test, it is necessary to reduce the time needed to obtain a perfectly...
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!
General
Article included in this offer
"Studies and properties of metals"
(
172 articles
)
Updated and enriched with articles validated by our scientific committees
A set of exclusive tools to complement the resources
Bibliography
References
Exclusive to subscribers. 97% yet to be discovered!
Already subscribed? Log in!